Dear All:
I have a Philips PW1800 and I want to know if anybody is using these type
of XRD to collect XRD patterns. I want to know the instrumental correction
to refine my patterns.
Best regards,
Ariel Bacci
I am using the software Quanto to quantify some "simple" patterns, mixes of
calcite and quartz.
I read a lot of information about Rietveld, but I have not enough
knowledgments about crystal structures, PO, etc.
I refined a pattern of 15% of quartz and 85% of calcite. I got a Gof of 1.9
using "Mod
Dear Maurizio:
How do you do? It is interesting to contact people who work in cement
industries!
Do you determinate clinker phases by XRD?
I want to know if you would detail me your method to prepare the samples
(standards and unknown ones).
I want to determinate CO2 because we add limestone
work in a cement company and I have a Philips XRD 1800. I want to
determinate quartz in limestone. I would like to deteminate CO2 in cements
and CaCO3 in limestone too. I am new in XRD utilization so I require
detailed answers.
Is another member who work in a cement industry?
Best regards