oops...
this wasn't for the list, just for Bob - sorry! Clarification: The comments on MAUD are of course related to HIPPO data - it works great, the comment on slowness relates to the mentioned triclinic texture where it took several days more than GSAS to get to a completed refinement. The
OOPS.
Sorry about that. ^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~^~ Peter W. Stephens Professor, Department of Physics and Astronomy Stony Brook University Stony Brook, NY 11794-3800 fax 631-632-8176