Hi everybody,
Could someboby send me the relative intensity and the peak position (2theta)
of the pyrochlore structure of the Gadolinium Zirconium Oxide (Gd2Zr2O7).
Thanks in advance.
ANGEL L. ORTIZ
Institute of Materials
Dear Jack,
Zirconia phases are all fluorite derivatives.
Cubic zirconia has the fluorite structure undistorted
(ie Fm3m, a=5.08 depending on the dopant species and temperature, Zr is at
0,0,0 and Oxygen at 1/4,1/4,1/4)
The tetragonal phase has space group P42/nmc with a=3.593, c=5.184, Zr at
3
oice
(847) 362-4871 Fax
> -Original Message-
> From: Jack Badenhorst [SMTP:[EMAIL PROTECTED]]
> Sent: Friday, October 30, 1998 8:23 AM
> To: [EMAIL PROTECTED]
> Subject: Zirconium oxide
>
> Hi everyone
> I need some help with the atomic positions for the follo
Hi everyone
I need some help with the atomic positions for
the following Zirconium Oxides.
1. Tetragonal (24-1164 , 42-1164, 17-0923) and
2. the cubic form
Can anyone help me?
Thanks
Regards Jack