Vilik; To make large particle CS use 380 vdc, 2"spacing, 3-1/2" immersion in 14 oz of water. The S.E.M. showed particles of 100 nanometer!!!! Time about one hour.
Robert -- The silver-list is a moderated forum for discussion of colloidal silver. To join or quit silver-list or silver-digest send an e-mail message to: [email protected] -or- [email protected] with the word subscribe or unsubscribe in the SUBJECT line. To post, address your message to: [email protected] List maintainer: Mike Devour <[email protected]>