12 days?  and only 99% gold?  Then I would suspect you might have a solution
of whatever the other 1% is.  Blue leads me to suspect maybe copper salts?

-----Original Message-----
From: Ivan Anderson <[email protected]>
To: Silver-List <[email protected]>
Date: Tuesday, October 26, 1999 5:12 AM
Subject: Re: CS>What am I making ?? c/gold


>The standard reduction potential of gold is Au ---> Au+++  +3e- 1.4
>volts
> or Au+ ---> Au+  + e-  1.69 volts
>So you will have a gold sol. I believe this can take a little time and
>you may be wise to limit the current, sounds the gold is burnt.
>
>Ivan.
>
>----- Original Message -----
>From: P Yanko <[email protected]>
>To: <[email protected]>
>Sent: Sunday, 24 October 1999 09:40
>Subject: CS>What am I making ?? c/gold
>
>
>> trying c/gold
>> A little bit of experimenting has produced a clear solution with a
>very
>> faint tinge
>> almost akin to a blue tropical lagoon.
>> .
>> 2 electrodes 99% Gold .7 mil dia 1' wetted. spacing 2.5mm, volts 36.
>Dc
>> current increased from 1ma
>> to 30 ma  after 12 days. hard black crud on electrodes, (had to
>scrape it
>> off) normal room temp (not heated water)
>> No fallout. using steam distilled water. no starter solution. no
>additives
>> good tyndall effect.
>>
>> Does anyone have any idea what I have made, I sure dont.
>>
>> P Yanko
>>
>>
>>
>>
>>
>>
>>
>> --
>> The silver-list is a moderated forum for discussion of colloidal
>silver.
>>
>> To join or quit silver-list or silver-digest send an e-mail message
>to:
>> [email protected]  -or-
>[email protected]
>> with the word subscribe or unsubscribe in the SUBJECT line.
>>
>> To post, address your message to: [email protected]
>>
>> List maintainer: Mike Devour <[email protected]>
>>
>