Subject: CS>electrode distance and Tyndall effect
Clear at three hours. Virtually no TE. RO Water. Start cold. On ssmall
hotplate. donut shaped magnet on hotplate north upward. One half gallon.
Electrodes half inch wide by 5 inches long by about 3 inches apart. 12 volt
transformer. Product has that distinctive metallic CS 'bite' My point???
Distance apart has a lot to do with a clear product. Usually I run it at 2
inches, it is usually somewhat stronger tasting but has a definite TE where
this batch almost totally lacks the TE. Del