Hi Nancy, Generally I find that clear CS can be made is the current density is keep about 1 ma/ sq in of wet electrode.
Do you have any meter readings on your process? What is the size, length, and number of anode electrodes are you using? Not cathodes !!! If you don't have a DMM then get one from Harbor Fraight of less than $5.00. With that if you measure the initial current when you start a batch. and that is about the best measure for the quality of DW and it will alert you to any changes in the water quality. "Ole Bob" -- The silver-list is a moderated forum for discussion of colloidal silver. Instructions for unsubscribing may be found at: http://silverlist.org To post, address your message to: [email protected] Silver-list archive: http://escribe.com/health/thesilverlist/index.html List maintainer: Mike Devour <[email protected]>