It's the cracks per Storms.  The reactions appear to occur at the
surfaces only.  In solid Pd, you have to saturate the crystalline
structure.  With high surface areas in Ni powder or Celani's treated
(cracked) wire, there is much more surface area so loading of the
total crystal is much less in play.

On Wed, Dec 12, 2012 at 9:31 PM, Mark Gibbs <[email protected]> wrote:
> And what about in the MFM Project?
>
> [m]
>
> On Wed, Dec 12, 2012 at 6:26 PM, Terry Blanton <[email protected]> wrote:
>>
>> Yes, McKubre takes the endothermic loading and exothermic off loading
>> into his calculations in his work at SRI.
>>
>> On Wed, Dec 12, 2012 at 9:17 PM, Mark Gibbs <[email protected]> wrote:
>> > Something I haven't seen any discussion about is the amount of energy
>> > required to load materials with hydrogen to be used in these various
>> > LENR/CF
>> > devices. If that energy is taken into account, are the claims of excess
>> > energy from the operation of the devices still valid?
>> >
>> > [mg]
>>
>