Here we are I've found some info, I just need someone to help me interpret it.

6061 T6  
Yield strength 275 mpa
Tensile strength 310 mpa
Elongation 12 %

5005 H34
Yield strength 140 mpa
Tensile strength 160 mpa
Elongation 8 %

Looks like the 6061 T6 is about twice as strong !!!! but given how much of it 
there is, I doubt strength is an issue.