Dear Rietvelders,
See below for three postdoctoral positions available within the Structural
Science Group here at the Advanced Photon Source
(http://www.aps.anl.gov/Xray_Science_Division/Structural_Science/).
Please distribute to anyone you think would be interested and a good match for
the pos
Dear Jae-Ho
The thermal parameters of the magnetic moments are identical to the
thermal parameters of the nuclei which they are attached to (along with
the x,y,z positions and occupancies). Normally they will refine much
better from the nuclear intensities which should extend to higher Q.
Be
Dear Rietvelders,
I have a question, particularly to experts in magnetic structure
refinements. When does one need to refine anisotropic thermal factors for
the magnetic moments? We have a set of data, on which we work hard to
extract physically meaningful magnetic structures. The intensities sugg