Marshall, Roger and Listers all,

I'd like to reply to the last para below:  I don't know of any SEMs that will 
resolve below 20 nm (nanometers); most are not better than 30 to 40 nm.  The 
accepted choice (of particle  characterization experts) for particles as small 
as those we are hopefully talking about here is TEM (transmission Electron 
Microscopy).  It's a real pity that it's not possible, because Scanning EM 
gives one a surface map and visual depth and TEM does not.  It would be so 
valuable to viualize the topography of these particles (and, as well, the 
crystalline structures one sees in HVAC products) in almost 3-D.  The best of 
TEMs will resolve to approx. one Angstrom (a tenth of a nm).   Why not ask the 
gentlemen to share such "studies". 

Stephen
  ----- Original Message ----- 
  From: Marshall Dudley 
  To: [email protected] 
  Sent: Tuesday, June 06, 2000 10:43 AM
  Subject: Re: CS>Re:HVAC-LVDC


  A great deal of information is found on this technique in The Formation of 
Colloids by The Svedberg, published by D. Van Nostrand Company 25, Park Place 
NY, 1921. 
  Marshall 

  [email protected] wrote: 

    In a message dated 00-06-05 23:41:46 EDT, you write: 
    << Subj:     CS>Re:HVAC-LVDC 
     Date:  00-06-05 23:41:46 EDT 
     From:  [email protected] (Fred) 
     Reply-to:  [email protected] 
     To:    [email protected] 

     Roger, have you found the Holy Grail? Is sputtering 25+ times more 
effecient 
     ("output increases by at least two orders of magnitude") then the 
relatively 
     loss less LVDC process? You and others often refer to "sputtering", the 
     definition which I know, (as in vacuum metalization) is the vaporization 
of a 
     metal (atoms, not ions?). Are you not then producing with sputtering a 
fine 
     suspension of silver particles? 

    Fred:  Yes, you are partially correct. I believe what happens during 
    sputtering is that the tip of the electrode becomes superheated well beyond 
    the melting point of silver, producing a significant silver vapor pressure 
    (At times I can see bubbles immerge from the surface of the molten silver 
    sphere at the electrode tip.) Then the fast moving ionized plasma collide 
    with the gaseous silver imparting a strong static charge as the silver 
atoms 
    are rapidly quenched into the water bath below so silver oxide is not 
formed 
    since (according to Ivan, and thermodynamics -- two equally reputable 
    sources) it is not stable above 150 degrees C. 

     Current density, in a real process,  is rarely the wetted surface area but 
     usually the projected surface area with maybe a 10-20% adder for fringe 
    effects. 

    Sounds about right Fred. I seem to have forgotten some of the finer points. 
    Well, electrometallurgy was my minor anyway. 

    As to the smaller particle size with the HVAC process, the LVDC process 
    releases 
     ions and they seem to come in only one size! What is your reference to 
HVAC 
     making smaller particles? 

    Well, Bruce Marx and David Ripley both claim to have SEM studies which show 
    that their HVAC CS particles are smaller then CONVENTIONALLY produced LVDC 
    CS. However, the type of LVDC CS produced by some "silver listers" (< 1 ma 
    max, with stirring in ONLY DW) could be quite a bit smaller in particle 
size 
    and distribution, I simply don't know. Secondly, if the mechanism above is 
    more or less correct, SPUTTERED HVAC CS should have a very small particle 
    size. 

    Roger 

    -- 
    The silver-list is a moderated forum for discussion of colloidal silver. 

    To join or quit silver-list or silver-digest send an e-mail message to: 
    [email protected]  -or-  [email protected] 
    with the word subscribe or unsubscribe in the SUBJECT line. 

    To post, address your message to: [email protected] 
    Silver-list archive: http://escribe.com/health/thesilverlist/index.html 
    List maintainer: Mike Devour <[email protected]>