Hi Ya'all,

This is the forst of a series of reports detailing my adventure with
submerged arc CS.

It is a "strange animal."

I have made two runs and a third is in progress now.

Ihave made a floating electrode assembly similiar to Bill Fernald's, but
question is that is necessary for silver as things havppen very fast,
and there is no evaporation of water. With gold that is another story
which will not be looked at for awhile.

The first batch was one gallon with equal sized electrodes using 12 kv
but it didin't work to well. Arc sustain problems. It looked like
regular HVAC ARC CS but had a bright red T.E. with no sparklies.

Batch #2 used one #14 and 0ne #18 silver with 6 liters of 0.22 uS/cc DW.
In 40 minutes I had a CS with a turpidity and color as Frank show on his
web site. The Spect reading was 5.17 ppm ionic with a conductance of
10.0 uS/cc.  After 24 hours the conductance was 7.7 uS/cc and the ionic
ppm was 2.42.

To test for particle content I placed 50 cc of CS in a test tube and add
5 cc of 35% H2O2. After several hours this was tested with the spec and
found an adjusted ppm for dilution with H2O2 to be 12.7 ppm.

I quess this says that sub-arc CS is 16% ionic and 84% particle.

I find it most interesting that both the ppm and conductance dropped
overnight.

Comments. Please,

"Ole Bob"


--
The silver-list is a moderated forum for discussion of colloidal silver.

To join or quit silver-list or silver-digest send an e-mail message to: 
[email protected]  -or-  [email protected]
with the word subscribe or unsubscribe in the SUBJECT line.

To post, address your message to: [email protected]
Silver-list archive: http://escribe.com/health/thesilverlist/index.html
List maintainer: Mike Devour <[email protected]>