Dan,

I don't give a d-mn what Pride Lbs say, but arcing gold in air is a disaster!!!!

Does you product have any color. Without a light violet color you do not have CG. I have done the design work and spent the money for the AA's to verufy my work. Without a lab analysis you aare being very foolish.

"Ole Bob" P.E.

[email protected] wrote:

Thanks. I shall ask Pride labs support. Arcing method goes much faster than
submersion of both electrodes. They prefer it.




--