cat,


I use 3M 77 spray for laminating paper and light card on to heavier material.

For thick material like illustration board I don't trust its long-term holding 
strength.



For small laminations I use the large disappearing purple Avery Glue Stick.




JoeG

-----Original Message-----
From: cat <[email protected]>
To: [email protected]
Sent: Thu, Aug 6, 2009 3:27 pm
Subject: [Papermodels II 39133] Re: START U-Boat Type VII-C 1:32









James Hairston wrote:
> If you use foam-core laminate both sides and lay it on a flat surface
> with a board on top until dry to prevent warping.

    Or use a low tack spray adhesive. All the warpage I have ever 
experienced were the fault of the adhesive not the process. After 
realizing the paper/card was not at fault I tried a number of adhesives 
and found the low tack ones  often found at art or drafting shops worked 
fine and the warping stopped.

                                cat





 





--~--~---------~--~----~------------~-------~--~----~
You received this message because you are subscribed to the Google Groups 
"Papermodels II" group.
To post to this group, send email to [email protected]
To unsubscribe from this group, send email to 
[email protected]
For more options, visit this group at 
http://groups.google.com/group/Papermodels?hl=en
-~----------~----~----~----~------~----~------~--~---

Reply via email to