> "Theoretically" U,V,W should not be refined at all as they describe instrumental > broadening
This is true only when there is no Gaussian strain present. Brian
> "Theoretically" U,V,W should not be refined at all as they describe instrumental > broadening
This is true only when there is no Gaussian strain present. Brian