Dear Nelson Duarte, Within the help system of HighScore Plus you will find various tutorial examples about Rietveld analyses. Just press the F1-key at any stage in the program to invoke the help system.
These tutorials will guide you step by step. In particular I would recommend you to look at the following chapters within the help file: 6. Analysis/Rietveld Analysis and 8. Practical/ Practice Rietveld analysis We tried to contact you personally by email, but have not yet received an answer. Please feel free to contact your local PANAlytical representatives at any time, they will help you further or will get you in touch with a specialist. Sincerely yours, Gwilherm Nénert Gwilherm Nénert - Product Marketing XRD PANalytical B.V. Lelyweg 1 (7602 EA) PO Box 13 7600 AA Almelo CoC Registration No. 06069492, Enschede, The Netherlands T +31 546 534 520 M +31 612726178 gwilherm.nen...@panalytical.com www.panalytical.com PANalytical get insight The information contained in this message is confidential and may be legally privileged. The message is intended solely for the addressee(s). If you are not the intended recipient, you are hereby notified that any use, dissemination, or reproduction is strictly prohibited and may be unlawful. If you are not the intended recipient, please contact the sender by return e-mail and destroy all copies of the original message. From: "Nelson" <nelson.dua...@ipn.pt> To: <rietveld_l@ill.fr>, Date: 09/05/2014 06:47 PM Subject: Quantification and rietveld refinement Sent by: rietveld_l-requ...@ill.fr Dear rietvelds I have some samples, all with the same two phases: alumina and crocoite (PbCrO4) (electrochemical bath). I use Cobalt radiation. Indexing, I use always the same two ICDD files, 74-0323 for alumina and 73-1332 for crocoite. I use software High score plus. Can i use the semiquantification of software for know the quantification of each phase betwen the samples. Wuhere i can find the right cif files for this two phases, for introduce in High score plus and made Rietveld refinement. Where i can find a manual or exemples of how to make a rietveld refinement of this XRD. I don´t have experience of rietveld analysis. Thanks in advances Best regrds Nelson++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++
++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++ Please do NOT attach files to the whole list <alan.he...@neutronoptics.com> Send commands to <lists...@ill.fr> eg: HELP as the subject with no body text The Rietveld_L list archive is on http://www.mail-archive.com/rietveld_l@ill.fr/ ++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++++