Hello all, Trem Williams sent me this message so I could review it for compliance with the non-commercial nature of the list. It's just fine by me, and I am forwarding it to you all because it is good info.
Constant current has been discussed and is thought to be among the best techniques we know about. But it hasn't been discussed a lot recently and it is good to get another developer's point of view. Thanks for good citizenship and for sharing your results, Trem. Be well, Mike D. >>>>>>>>>>>>Begin included message Hello All, I have to jump in and pass on some information we have regarding voltage, current density, current flow, timing, water temperature, electrode spacing, electrode immersion depth and electrode deterioration. We use 1/4" wide by 5" long silver electrodes with our colloid generators. This results in quite a large surface area of silver. Immersion depth is about 3 inches, typically. Our generators limit the current with a regulator to a constant, low current value so as to get very low current density. We do not get any bubbling, boiling or any odd looking effects. Just a slow release of silver into the water. Our instructions are to not use saline, do not heat the water, use steam distilled water and place the electrodes at least two inches apart. Nothing critical there. We suggest running the unit for 4-5 hours in 16 ounces of water to get 15-20 PPM. As you can see, our generators take quite some time to make a batch but what is a little extra time when the results are always the same. We are able to get repeatable results every time a batch is made. All the variables are taken care of by using the constant current regulator. Spacing and water temperature are not part of the equation. All one has to do is use the same amount of distilled water and run the generator for the same time to get the same results each time. It's a no brainer. The key here is CONSTANT CURRENT. As far as I'm concerned, using a constant voltage source is the same as trying to drive a car with the gas pedal stuck to the floor. The speed is going to continue to increase until the engine is turned off. The same analogy applies to using constant voltage. Wire spacing, size, depth of immersion and water temperature are the variables and when the silver starts to build up in the water, the current starts to run away and increase too rapidly. That's why it bubbles, makes black particles, gets brown, etc. And it is almost never repeatable. There are too many variables in the process using a constant voltage source. If one wants to do it inexpensively without using electronic circuitry to make it automatic, try using a rheostat and milliameter in series with the battery and electrodes. These are available at Radio Shack or any electronic parts store. After the current starts to flow, adjust the rheostat to maintain current at some low value. In our case we adjust the internal regulator so that it maintains a constant current flow of 1 milliampere. I would suggest that value for the do-it-yourselfers if they use electrodes with equivalent surface area to our electrodes. If using wire, the surface area will be less and the current density will be higher so I can't suggest what current to use. I would suggest a lower value. It is our experience that the electrodes will last upwards of 700-1000 hours if they are reversed every once in a while. It is also our experience that there is little or no sludge or fallout using this technique. Particle size is small as attested to by consistently clear colloidal water without any "sparklers" when a laser is shone through the water. The color is golden and depth of color is determined by length of running time. It is never cloudy; always clear. It is never brown, purple, blue or red. Just light golden, clear water. The upshot is; use more silver surface area and limit the current and you will get repeatability. And that's what we're all after isn't it; a uniform product? Good luck to all. Trem Williams www.silvergen.com -----Original Message----- From: Pam Whitmire <[email protected]> To: [email protected] <[email protected]> Date: Monday, June 28, 1999 8:15 PM Subject: CS strength, times, etc. >Ok, I'm confused. Someone told me that you don't WANT to see your silver >wires bubbling and misting. And NOT to use saline. When I used saline, I >saw lots of mist rising off one of the wires (I'm using a small >generator with 3 9volt batteries) and the solution stayed sort of misty. >Tasted just like the gold-colored CS that I had bought from a company. >When I didn't use saline, I didn't see anything at all happening. Does >it take a lot of time? One article said DONT boil the water - another >said DO boil it. Today I heated the water to approx. 125 degrees, >started the generator and at about 11 minutes I began to see tiny >bubbles on one rod. Started timer again, and at the end of about 24 >minutes the one rod was black and starting to form some deposits on the >end (but none were dropping in the water) the other rod was also >blackish and beginning to mist a bit from the end. I turned it off and >have left it alone. How do I know it's correct? Do you just assume that >you got a good solution because you had the water, silver, generator and >left it for x amount of time? I know I sound like a real dummy, but I >really want this to work for me. I appreciate all of you who have taken >time to answer me....feel free to reply to me personally if that is >best. Thanks in advance, >Pam -- The silver-list is a moderated forum for discussion of colloidal silver. To join or quit silver-list or silver-digest send an e-mail message to: [email protected] -or- [email protected] with the word subscribe or unsubscribe in the SUBJECT line. To post, address your message to: [email protected] List maintainer: Mike Devour <[email protected]>

