Reid Harvey wrote:

> Marshall,
> Now I'm rereading the last part of your message, and it sounds as if
> this is another good suggestion, using AgNO3 with cafeine, along with
> some other silver already present.  Just a couple of questions and
> observations:
>
> If the first silver in the purifier medium were the nitrate, fired then
> going to metal, it seems the particles would be very small.  By contrast
> I'm thinking that if using CS the particles may be a lot bigger,
> something like 100 nanometers.  This difference wouldn't seem all that
> important to me, given that lots of things have worked as disinfectant
> so far, various forms of silver and different particle sizes.  But in
> these several scenarios, if doing additional treatment with the nitrate
> then the caffeine, then enlarging particle size, what would then be the
> various implications?  For one thing, according to what you're saying
> the existing particles will get bigger, no additional particles
> forming.  So far I'm not seeing clearly and maybe a few days of thought
> will help.
>

That is correct. If you could start out with silver atoms, then built them
up to small particles that might work very well.

>
> A novel prospect would appear to be first saturating with the density of
> particles desired, albeit small particles, then growing these particles
> in the second treatment, to an optimal size.  But while it sounds good
> on paper I'm hard put to think what those optimal densities and optimal
> sizes would be.

You are correct. I am giving you this information based on photographic
developing science, and in practive it is theory only.  I have no idea what
if anything the clay or other impurities may do.

As far as caffine being a developer, see
http://www.rit.edu/~andpph/text-coffee.html

Marshall

>
> Reid
>
> Marshall Dudley said:
> .........I still think that a mixture of CS, silver nitrate, and a
> developer could do wonders.  Have you tried that?  The CS
> would provide silver atoms/particles for the silver in the silver
> nitrate to plate out on, and the developer (even
> caffine works if you keep the ph right), will cause the silver to plate
> out onto the particles over a few minutes
> time.
>
> A way to do this without having to mix up a new batch each time would be
> to saturate the unit with CS, or put it
> in the original mixture before firing. Then once it is dry, slowly force
> a mixture of silver nitrate and developer
> through it.  When the silver crystals are as large as you want (the
> whole thing should turn grey then black as the
> crystals increase in size), flush with clean water to remove the
> developer and silver nitrate.  If you let it sit 15
> minutes or so, then most of the silver nitrate should reduce, thus
> reducing wasted silver.  Be sure to pick a
> developer that you can either completely wash out, or one that is
> non-toxic.  I think caffine may be a good
> choice for that since it is pretty well non-toxic.
>
> For additional insight on this, I suggest researching photo developing
> techniques.
>
> Marshall
>
> --
> The silver-list is a moderated forum for discussion of colloidal silver.
>
> Instructions for unsubscribing may be found at: http://silverlist.org
>
> To post, address your message to: [email protected]
>
> Silver-list archive: http://escribe.com/health/thesilverlist/index.html
>
> List maintainer: Mike Devour <[email protected]>