The way I see it is that the effects of silver on microbes depends on
'available' surface area.
In a liquid, that surface area can be huge depending on the size of the
particles.
In a solid, it will be limited by the exposure possible at a given
porosity...that is, the size of the pore in the filter will determine the
maximum exposure of silver to the water going through it by the surface
area presented by the pore.
The best you can do is to make very small pores entirely coated with silver.
The silver that's not on the pore surface will do nothing at all.
If it's possible to make tiny, close packed but still seperate beads of
silver on the pore surface, THAT may increase surface area exposure over a
solid sheet.
So, "possibly", saturating the filter with oxide particles small enough to
get into the pores and burning off the oxygen in the oxide during fireing
will make those micro beads that stay stuck to the clay surface.
If you're using sawdust to determine the size of the pore in the clay,
perhaps soaking the sawdust with silver oxide sludge will do it. [Or
specifically sized...by screening?... charcoal chunks?]
It's not hard to make CS sludge. [Lots of voltage and current and enough
time to disintigrate the electrode..done wrong the right way, mere minutes.
Guessing 20,000 volts at a few amps?]
If voltage and current is high enough, the sludge will actually emulsify.
It will be deep brown turning to quite black.
{ I discovered the best way to not make good CS first off...slight fire
hazard there too.}
Patterson [forget the first name...James?] patented micro beads and made
millions when it became apparent that they had unique delivery properties
for many cosmetics and drugs depending on what the bead coating was.
Many products you buy today have that feature.
Patterson is the guy who now is playing with a cold fusion process that
uses micro beads. [Microscopic round particles coated with another
material...palladium?]
This will be too high tech to do in the field, but it seems like spraying
very fine clay dust [or silica to make glass beads?] into a vaccuum along
with a silver plasma will result in such a bead which then could be
pressure packed or sintered together to form a pourous shape.
I've seen various filters [especially fuel filters] made by packing small
round metallic shapes together..perhaps bonded by heating them to the point
of stickyness [like spot welding] or perhaps simply by applying large
amounts of pressure in a mold. The size of the bead and extent of the
packing effect determines the porosity.
Ode
At 02:40 PM 11/17/2003 -0500, you wrote:
>Reid Harvey wrote:
>
>> Marshall,
>> Now I'm rereading the last part of your message, and it sounds as if
>> this is another good suggestion, using AgNO3 with cafeine, along with
>> some other silver already present. Just a couple of questions and
>> observations:
>>
>> If the first silver in the purifier medium were the nitrate, fired then
>> going to metal, it seems the particles would be very small. By contrast
>> I'm thinking that if using CS the particles may be a lot bigger,
>> something like 100 nanometers. This difference wouldn't seem all that
>> important to me, given that lots of things have worked as disinfectant
>> so far, various forms of silver and different particle sizes. But in
>> these several scenarios, if doing additional treatment with the nitrate
>> then the caffeine, then enlarging particle size, what would then be the
>> various implications? For one thing, according to what you're saying
>> the existing particles will get bigger, no additional particles
>> forming. So far I'm not seeing clearly and maybe a few days of thought
>> will help.
>>
>
>That is correct. If you could start out with silver atoms, then built them
>up to small particles that might work very well.
>
>>
>> A novel prospect would appear to be first saturating with the density of
>> particles desired, albeit small particles, then growing these particles
>> in the second treatment, to an optimal size. But while it sounds good
>> on paper I'm hard put to think what those optimal densities and optimal
>> sizes would be.
>
>You are correct. I am giving you this information based on photographic
>developing science, and in practive it is theory only. I have no idea what
>if anything the clay or other impurities may do.
>
>As far as caffine being a developer, see
>http://www.rit.edu/~andpph/text-coffee.html
>
>Marshall
>
>>
>> Reid
>>
>> Marshall Dudley said:
>> .........I still think that a mixture of CS, silver nitrate, and a
>> developer could do wonders. Have you tried that? The CS
>> would provide silver atoms/particles for the silver in the silver
>> nitrate to plate out on, and the developer (even
>> caffine works if you keep the ph right), will cause the silver to plate
>> out onto the particles over a few minutes
>> time.
>>
>> A way to do this without having to mix up a new batch each time would be
>> to saturate the unit with CS, or put it
>> in the original mixture before firing. Then once it is dry, slowly force
>> a mixture of silver nitrate and developer
>> through it. When the silver crystals are as large as you want (the
>> whole thing should turn grey then black as the
>> crystals increase in size), flush with clean water to remove the
>> developer and silver nitrate. If you let it sit 15
>> minutes or so, then most of the silver nitrate should reduce, thus
>> reducing wasted silver. Be sure to pick a
>> developer that you can either completely wash out, or one that is
>> non-toxic. I think caffine may be a good
>> choice for that since it is pretty well non-toxic.
>>
>> For additional insight on this, I suggest researching photo developing
>> techniques.
>>
>> Marshall
>>
>> --
>> The silver-list is a moderated forum for discussion of colloidal silver.
>>
>> Instructions for unsubscribing may be found at: http://silverlist.org
>>
>> To post, address your message to: [email protected]
>>
>> Silver-list archive: http://escribe.com/health/thesilverlist/index.html
>>
>> List maintainer: Mike Devour <[email protected]>
>
>