On Mon, 7 Mar 2016 10:23:31 +0800
TJoseph Powderly <[email protected]> wrote:

> off time is really dpendant on flushing conditions
> on time causes rougher finer surface finish

I guess this explain it all and it also make perfect sense. More powder behind 
remove more material and longer time in between leave more time for debri to 
remove debri.


Regards Nicklas Karlsson

------------------------------------------------------------------------------