That is correct.

Marshall

[email protected] wrote:

> Marshall
>
> I noticed the "F" after 32 this time. That means you're making CS slightly
> above freezing, yes?
>
> In a message dated 10/04/1999 6:11:22 PM Pacific Daylight Time, [email protected]
> writes:
>
> << t is our experience that heating the water results in the motion of the
>  particles being able to overcome the mutual repulsion of the particles and
>  thus leads to aggregation, and larger particle size.
>
>  That is why we make ours at just above 32 F.  I can state for a fact that in
>  our process that if it is made at room temperature or at elevated
> temperature,
>  the particle size is significantly larger.  However our process does differ
>  from the DC process since we are using HVAC and a microflow process.  I would
>  think that this would be the same for the DC process, but have not tested it.
>   >>
>
> --
> The silver-list is a moderated forum for discussion of colloidal silver.
>
> To join or quit silver-list or silver-digest send an e-mail message to:
> [email protected]  -or-  [email protected]
> with the word subscribe or unsubscribe in the SUBJECT line.
>
> To post, address your message to: [email protected]
>
> List maintainer: Mike Devour <[email protected]>