Hi I would avoid super heat type approaches. The risk is getting the glass to metal seals on the base to hot to fast. Normally the can needs more heat than the base, but not always. A lot depends on just how thick each one is and what they are made of.
Bob -----Original Message----- From: time-nuts-boun...@febo.com [mailto:time-nuts-boun...@febo.com] On Behalf Of Stan, W1LE Sent: Thursday, February 09, 2012 7:47 AM To: Discussion of precise time and frequency measurement Subject: Re: [time-nuts] Morion MV89 output level? Would it be better to apply heat the metal shell or to apply heat the bottom part with the I/O pins ? I would start using a propane gas torch. Heating quickly till I saw the solder flow. Stan, W1LE Cape Cod On 2/9/2012 6:04 AM, Azelio Boriani wrote: > Don't be afraid and open up your MV89. I have done this with many MV201 > without problems. > > _______________________________________________ time-nuts mailing list -- time-nuts@febo.com To unsubscribe, go to https://www.febo.com/cgi-bin/mailman/listinfo/time-nuts and follow the instructions there. _______________________________________________ time-nuts mailing list -- time-nuts@febo.com To unsubscribe, go to https://www.febo.com/cgi-bin/mailman/listinfo/time-nuts and follow the instructions there.